bigdog007,
Not sure which code you are referring to but as weldtek has stated
ASME VIII - UW 37
(f) Welder and Welding Operator Identification
(1) Each welder and welding operator shall stamp
the identifying number, letter, or symbol assigned by
the Manufacturer, on or adjacent to and at intervals
of not more than 3 ft (0.9 m) along the welds which
he makes in steel plates 1?4 in. (6 mm) and over in
thickness and in nonferrous plates 1?2 in. (13 mm) and
over in thickness; or a record shall be kept by the
Manufacturer of welders and welding operators employed
on each joint which shall be available to the
Inspector.
Also,
B31.1 - 127.6
The WPQ shall also show the identification symbol
assigned to the welder or welding operator employed
by him, and the employer shall use this symbol to identify
the welding performed by the welder or welding
operator. This may be accomplished by the application
of the symbol on the weld joint in a manner specified by
the employer. Alternatively, the employer shall maintain
records which identify the weld(s) made by the welder
or welding operator.
B31.3 - 328.5
(b) Each qualified welder and welding operator shall
be assigned an identification symbol. Unless otherwise
specified in the engineering design, each pressure containing weld or adjacent area shall be marked with the
identification symbol of the welder or welding operator.
In lieu of marking the weld, appropriate records shall
be filed.
Hope this helps,
Cheers,
Kiwi