Jul 15, 2010 #1 albaweld Petroleum Joined Jul 23, 2007 Messages 29 Location CA As per Sec IX, if a welder is qualified by using a production weld, is that welder only qualified for that particular project or can that qualification be used for further projects, all process parameters the same?
As per Sec IX, if a welder is qualified by using a production weld, is that welder only qualified for that particular project or can that qualification be used for further projects, all process parameters the same?
Jul 15, 2010 #2 JStephen Mechanical Joined Aug 25, 2004 Messages 8,736 Location US The welder is qualified for other projects, within the range of parameters specified. Upvote 0 Downvote
Jul 15, 2010 Thread starter #3 albaweld Petroleum Joined Jul 23, 2007 Messages 29 Location CA thank you... Upvote 0 Downvote