Hi All,
We have ordered one Drilling Tool (Whipstock) which should be made of single piece Tubular mandrel. But supplier has come up with a deviation request that the supplied Tool will be of welded type instead of single body type due to concave curvature configuration & associated machining difficulties. . In this case, the two sections of steel plates will be rolled & welded together (butt weld) to form a single assembly.
We requested for additional documents such weld map, WPS and NDE procedures.
Considering design changes (single piece v/s welded), do need to request for any design analysis documents (ex: FEM analysis) or MOC to mitigate any risks in drilling wellbore condition?
Thank you in advance.
We have ordered one Drilling Tool (Whipstock) which should be made of single piece Tubular mandrel. But supplier has come up with a deviation request that the supplied Tool will be of welded type instead of single body type due to concave curvature configuration & associated machining difficulties. . In this case, the two sections of steel plates will be rolled & welded together (butt weld) to form a single assembly.
We requested for additional documents such weld map, WPS and NDE procedures.
Considering design changes (single piece v/s welded), do need to request for any design analysis documents (ex: FEM analysis) or MOC to mitigate any risks in drilling wellbore condition?
Thank you in advance.