I personally have not needed to specify WP91 fittings at any of our Power Plants. This material is permitted, however, for use as fittings in accordance with ASME B16.9, SA-234 Grade WP91.
Be aware of specific welding requirements for using WP91 material - proper selection of filler metal, preheat and post weld heat treatment requirements.