Hi!

Can I weld coil nuts to the plate to make precast concrete connections?

JRW
 
This needs a bit more context

You -may- be able to do so, but be very careful - some types of bolt steel (including nuts and washers) is NOT weldable and you will irreparably degrade your connection by welding the wrong types of steel
 