ASTM A234 WPB pipe fitting have a Cmax content of 0.3 and a Ceq of 0.66 corresponding to the max range of the constituents. There are specs requiring the C content limited to 0.23 and Ceq to 0.42 so as to provide weldability. Will the weldability become a problem if the C content comes close to the upper ranges of the WPB constituents.
 
Replies continue below

Recommended for you

No, preheat and hydrogen control of weld rod become necessary to avoid delayed cracking.
 