nilaypathak
Civil/Environmental
All structural weld requires 100% visual inspection. Our subcontract shop and company CWB certify company. They are going to do structural field welding. As per code requirement welding shall be done by certified inspector or qualify or experienced person approved by engineer.as per W59.
Subcontractor will do 100% visual inspection but it always done by welder who does welding. Subcontractor do not agree that visual inspection shall be done by other, not the welder.
EOR(Engineer of Record) stated in the situation that visual inspection requires for all structural welding and full penetration welding requires NDT.
Our QA manager do not approves the ITP of subcontractor because visual inspection are not going to done by certified welding inspector.
There are the three sides. I would like to request your for the situation for How should I close this issue.
Please share Standard procedure for visual inspection.
Thank you for your time.
Subcontractor will do 100% visual inspection but it always done by welder who does welding. Subcontractor do not agree that visual inspection shall be done by other, not the welder.
EOR(Engineer of Record) stated in the situation that visual inspection requires for all structural welding and full penetration welding requires NDT.
Our QA manager do not approves the ITP of subcontractor because visual inspection are not going to done by certified welding inspector.
There are the three sides. I would like to request your for the situation for How should I close this issue.
Please share Standard procedure for visual inspection.
Thank you for your time.