Can somebody help me in calculating the weld strength of a 20" SCH 80 pipe connected perpendicular to a 42" diameter, 9 mm thick (not seamless) pipe, SS304 material. It has a reinforcing pad of CS material of 9 mm thickness.The 42" diameter run is installed vertically and is heated to 600 deg C. On my actual measurement, maximum deflection of the 20" diameter pipe wrt x-axis from the support, due to linear thermal expansion of the 42" diameter pipe, is 60 mm.
We would like to increase the operating temperature of the assembly to about 750 deg C. I am worried that the welds on the tie point will not anymore carry the stress induced by thermal expansion.
We would like to increase the operating temperature of the assembly to about 750 deg C. I am worried that the welds on the tie point will not anymore carry the stress induced by thermal expansion.