A recent project has a SS base plate welded to an HSS column.
Can someone suggest a procedure and the type of welding to achieve that? or would regular SS welding procedures and electodes be adequate? The Hilti SS anchors will be covered with a SS cover; should the weld be passivated? Thanks in advance. Normal spec is:
-STAINLESS STEEL WELDING SHALL CONFORM TO ANSI/AWS D1.6-2017.
-WELDING ELECTRODES MAY BE 308L.
Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?
-Dik
Can someone suggest a procedure and the type of welding to achieve that? or would regular SS welding procedures and electodes be adequate? The Hilti SS anchors will be covered with a SS cover; should the weld be passivated? Thanks in advance. Normal spec is:
-STAINLESS STEEL WELDING SHALL CONFORM TO ANSI/AWS D1.6-2017.
-WELDING ELECTRODES MAY BE 308L.