Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Weld shape

Status
Not open for further replies.

fjodor

Mechanical
Joined
Aug 13, 2012
Messages
20
Location
HR
Hi,
Can someone share examples of weld shape between connector and shell at an angle like on the image:
2rdaw04.jpg


thx in advance
 
The first thing I see is that the nozzle to shell joint is not a fillet weld. The weld is a complete joint penetration groove weld with the joint geometry changing around the circumference.

The configuration of the groove, as shown, at the top of the sketch is nearly impossible to weld due to the limited access and the narrow groove angle. As a minimum, the groove angle at any point should be no less than 60 degrees, better yet if it is about 70 degrees.

The butt joint between the weldneck and the nozzle is a standard V-groove. Per B16.25 the groove angle should be 75 degrees and the weld should be complete joint penetration.

Best regards - Al
 
Exactly, that is the main problem, angle is afwul. In ASME VIII there is an example of similiar problem and it's hanled like on the image, basically nozzle is welded like weldolet.
 