May 19, 2018 #1 nkvon Petroleum Joined Nov 16, 2008 Messages 18 Location VN Dear All, My company is fabricating casing: plate 6 mm weld to stiffener(angle and bar) as file attached, Please help me welding sequence to minimize distortion, we use FCAW process, Thank you first, https://files.engineering.com/getfile.aspx?folder=c1876a10-58d3-4173-90c2-d7b4f2ad1725&file=Plate_vs_Stiffener.jpg