Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Weld Repair in the SAW weld seam of Spiral Steel Pipe

Status
Not open for further replies.

Godoy

Materials
Joined
Mar 3, 2015
Messages
5
Location
BR
Is Allowable to do a weld repair in defect type melt througth,using qualified FCAW process?
 
Most likely not. I would reject it.
Far better to cut it out.

OMG%20something%20else.png
 
Tks BigInch, we will consider your recomendation to stutus definition of pipes with this type of defective welds.
 