We have an exchanger shell plate A335 P12 15mm thick that was internally weld overlaid by flux wire process using a wire TP430.
After weld the clad deposition of TP 430, the dye penetrant inspection revealed that TP430 weld overlay was found with lots of pores and cracks.
What went wrong in this welding procedure?
Wrong filler wire?
Lack of PWHT?
Will it be beneficial to use of TP410S filler metal instead of TP430?
Thanks