engr2GW
Petroleum
- Nov 7, 2010
- 308
Hi,
I have two WPS,
1. First one qualified with 2" 0.218 coupon, from QW451.1 for weld metal thickness and base metal thickness, this coupon falls into the base metal range of 1/16" to 2T (0.436"), and the weld metal max. is 2t, does that mean that the range for the weld metal is 1/16" to 2t also? in other words, what's the minimum for the weld metal range and is 2t=2T?
2. and the other with an 8" 0.500" coupon, from QW451.1 for weld metal thickness and base metal thickness, this coupon falls into the base metal range of 3/16" to 2T (1.000"), and the weld metal max. is 2t, does that mean that the range for the weld metal is 3/16" to 2t also? in other words, what's the minimum for the weld metal range and is 2t=2T?
Thanks a lot.
I have two WPS,
1. First one qualified with 2" 0.218 coupon, from QW451.1 for weld metal thickness and base metal thickness, this coupon falls into the base metal range of 1/16" to 2T (0.436"), and the weld metal max. is 2t, does that mean that the range for the weld metal is 1/16" to 2t also? in other words, what's the minimum for the weld metal range and is 2t=2T?
2. and the other with an 8" 0.500" coupon, from QW451.1 for weld metal thickness and base metal thickness, this coupon falls into the base metal range of 3/16" to 2T (1.000"), and the weld metal max. is 2t, does that mean that the range for the weld metal is 3/16" to 2t also? in other words, what's the minimum for the weld metal range and is 2t=2T?
Thanks a lot.