Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Weld joint FEA - ASME VIII-1 vessel

Status
Not open for further replies.

jakov11000

Mechanical
Joined
Feb 24, 2016
Messages
20
Location
CA
Hello,

The vessel is designed as ASME VIII-1. Special Loose Type Flange (Seal Ring) is welded to the shell. The applicable code sketch, for welded joint size, would be Figure 2-4 sketch (3a). Due to special design of the seal ring (the Loose Flange) we cannot provide weld throat of min.=0.7*c as specified on Figure 2-4 (3a). Therefore the FEA is performed, to validate the weld strength. How do we validate the FEA results? That is, what allowable stress should be used? What kind of stress (membrane, bending, shear, membrane + bending) should be checked in the FEA?



Thank you!
 
 https://files.engineering.com/getfile.aspx?folder=05b21930-90b6-4a7f-adbb-bacdae527b7c&file=Welded_joint_flange_to_shell.png
If there are mandatory provisions in Section VIII, Division 1, you cannot overrule them with FEA.

Nevertheless, please refer to the 2019 Edition, Appendix 46.
 