Dear all, good night to everybody,
we have a case downstream christmas tree for oil production 8" 2500 rating where is required 10D of cladded pipe for chemical corrosion inhibitor injection.
After 10D of cladded material ( LTCS + 3 mm of ALLOY ) is request to change to Carbon steel 2500rating 8".
The question is : it is possible to weld cladded matarial with carbon steel material?
Which is the code that instruct how to weld this two material? which is the process?
There is some process to follow in order to weld the 2 material?
Since a couple of flange is not permitted I need to found a solution how to weld the 2 material.
Client have request 10 D after cladded material before the first welding point on carbon steel due to GALVANIC corrosion.
( but in my opinion is not real since we have carbon steel also after the cladded portion )
But not every place is permitted due to layout constrain.
In my mind I have this case :
1)Remove cladded material from cladded piping is not permitted since the remaining tickness is not design for design pressure.
2)Add some 200 mm of cladded material in carbon steel piping spool and weld with incoloy material
3)make a spool half cladded and half not from clad vendor.
Thanks a lot for the cooperation.
Best Regards
we have a case downstream christmas tree for oil production 8" 2500 rating where is required 10D of cladded pipe for chemical corrosion inhibitor injection.
After 10D of cladded material ( LTCS + 3 mm of ALLOY ) is request to change to Carbon steel 2500rating 8".
The question is : it is possible to weld cladded matarial with carbon steel material?
Which is the code that instruct how to weld this two material? which is the process?
There is some process to follow in order to weld the 2 material?
Since a couple of flange is not permitted I need to found a solution how to weld the 2 material.
Client have request 10 D after cladded material before the first welding point on carbon steel due to GALVANIC corrosion.
( but in my opinion is not real since we have carbon steel also after the cladded portion )
But not every place is permitted due to layout constrain.
In my mind I have this case :
1)Remove cladded material from cladded piping is not permitted since the remaining tickness is not design for design pressure.
2)Add some 200 mm of cladded material in carbon steel piping spool and weld with incoloy material
3)make a spool half cladded and half not from clad vendor.
Thanks a lot for the cooperation.