Hi everyone,
i have to do some weld strength calculation with which i don't have any experience. i am using EN1993-1-8 to guide me, but i have 2 questions:
1. in section 4.5.3.2 item 6, can anyone tell me what gamma_M2 is, that is used in the strength criterion of a fillet weld?
2. in the same criterion beta_w is used. values are listed for steel types, but i have to calculate welds in a stainless steel structure. how can i find the beta_w values for AISI316L? or should I be using a different spec?
Thanks!
Mark
i have to do some weld strength calculation with which i don't have any experience. i am using EN1993-1-8 to guide me, but i have 2 questions:
1. in section 4.5.3.2 item 6, can anyone tell me what gamma_M2 is, that is used in the strength criterion of a fillet weld?
2. in the same criterion beta_w is used. values are listed for steel types, but i have to calculate welds in a stainless steel structure. how can i find the beta_w values for AISI316L? or should I be using a different spec?
Thanks!
Mark