Hi,
is it allowed to perform weld build up repair on the inner side of a torispherical head in the knuckle region.
The defective area is localised,its overall diameter 15mm, extending to cca 1/3 of the original wal thickness.
The vessel is horizontal, cylindical, Ø 2100 mm, volume 30 m³, used for LPG storage.
All repair activites would be performed under pertaining codes and standards.
kind regards
Janos

 
Replies continue below

Recommended for you

If "All repair activites would be performed under pertaining codes and standards" then it is allowed.

Regards
r6155
 