Hello there,
Metal loss occurred on nozzles during construction activity. There are approximately 1/32" on nozzle 1, 1/16" on nozzle 2, 3/32" on nozzle 3. Looking for a repair procedure in order to meet minimum wall thickness.. nozzles are carbon steel material....
Appreciated help in advance.....
 
Dear RP535,

Are you talking about nozzles on a vessel being fabricated in a shop?

Or is it about nozzles on a vessel being welded in the field?



DHURJATI SEN
 
Thanks, David..
Hello Sen,
It was shop fabricated at shop, ship to field, construction contract made a mistake like I explained earlier..
 