Reformed Gas TO Synthesis Gas Convertor Reactor - Shell Plate SA 516 Gr 55 Material - Weld Hardness 243 Brinells Hardness / HAZ 226 Brinells Hardness. ASME SEC II Part C (welding consumables)SFA 5.1 Specification for carbon steel electrodes for Shielded metal arc welding dosen't mention WELD & HAZ harness values. During Plant ShutDown the equipment welds and HAZ hardness values taken by digital harness tester and values recorded. Now these values to be verified against the Fabrication code speficifed values. where can i find the hardness values specified by industrial codes /standards
If in case values are higher than the specified by farication code ASME Sec VIII Div 1. what is possible remedial action to be taken for Reactor Life integrity.
Similarly for P3 material Hardness of Reformer Headear values, as given in ANSI B 31.3 is 225 BHN . And the recorded values on the equipment are higher than the specified by the standard. What is the Remidial measure for the Header life integrity.
WELD & HAZ Recorded Values Attached.
If in case values are higher than the specified by farication code ASME Sec VIII Div 1. what is possible remedial action to be taken for Reactor Life integrity.
Similarly for P3 material Hardness of Reformer Headear values, as given in ANSI B 31.3 is 225 BHN . And the recorded values on the equipment are higher than the specified by the standard. What is the Remidial measure for the Header life integrity.
WELD & HAZ Recorded Values Attached.