In some cases there is only weight loss, if the corrosion products are soluble.
This is often true of Cu corrosion.
Also in some cases of very localized corrosion (pitting) the weight change may be very small and hard to detect by weight.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed