Hi ,

Good day.

I'm not familiar with WEDM .

I just want to ask if you have sample post for WEDM Fanuc.

As of now, the post that is default in NX are mitsubishi, agie and charmilles that are quite different on Fanuc.

This is the sample from other software.

(FIG#1 / CONTOUR - 1)
G54
G90G00X-1.Y-17.
M00
M37B15
M89
S1D1G04X2.
M15P0
G92
G90G01G41X-1.Y-18.
X0.
X1.
Y0.
X15.
Y-18.
X16.
X17.M00
G40Y-17.
G04X5.
M00

(FIG#1 / CONTOUR - 2)
G54
G90G00X17.Y-17.
M38B15H0
M88
S2D2G04X2.
M15P0
G92
G90G01G42X17.Y-18.
X16.
X15.
Y0.
X1.
Y-18.
X0.
X-1.
G40Y-17.
/M50
G54
G90G00X0.Y0.
M30
%


Thank you in advance.


mj
 