Hey folks:
You did such a good job answering my last question, I thought I'd ask another.
The "weaving" technique. How many electrode dia (using SMAW) and why? Does this apply to all other manual and semi automatic welding processes?
Thanks
Sftyvlv
 
Replies continue below

Recommended for you

Your question is too open ended. Weaving technique can be and is often employed for automatic, semiautomatic and manual GTAW, SMAW, GMAW, FCAW processes.

 