Amear
Mechanical
- Dec 6, 2004
- 12
Would anyone be kind enough as to tell me the min and max dia for a M20x2.5 7H and 8H minor diameter. Tons of trouble looking for this information. Below is all Ive been able to come up with.
-
-
Internal Metric Thread- M Profile Limiting Dimensions, ANSI/AMSE B1.13M-1983 (R1995)
-
-
Basic thread minor diameters D1
designation min max
M20x2.5 6H 17.294 17.744
-
Material is too hard and is wearing out our taps too fast, Im looking to use a larger drill that will hopefully meet the 7H or 8H specs, which I have yet to find. All thanks appreciated.
Alex
London ON
-
-
Internal Metric Thread- M Profile Limiting Dimensions, ANSI/AMSE B1.13M-1983 (R1995)
-
-
Basic thread minor diameters D1
designation min max
M20x2.5 6H 17.294 17.744
-
Material is too hard and is wearing out our taps too fast, Im looking to use a larger drill that will hopefully meet the 7H or 8H specs, which I have yet to find. All thanks appreciated.
Alex
London ON