In the company that i work for, we melt the sulfur using a coil made from ASTM A-53 Gr B. This Coil last 1 month. We tried with AISI 304 but with the same results. Anyone know about a material that last more than 6 months.

I read about the AISI 310 . What do you think?
 
Replies continue below

Recommended for you

310 should have at least five times the longevity of 304.
 