I require 1 piece gate valve with WC1 material, but my manufacturer is offering WC6 as he is finding it difficult to procure WC1 for just 1 piece. Could any one advise me if I can accept WC6 in place of WC1
 
Dear hsbcn, the only info I have is that this valve is intended for Water Oil & Gas service. Please advise.
 
Dear hsbcn, there are no details about pressure/temp
 