Hi,
Anyone knows a material with which and how I can manufacture a waterproof polymeric fabric for lightweight foldable raincoats.My first time, so excuse me if I haven't done this right.
Thanks.
 
Goretex

TTFN

Eng-Tips Policies FAQ731-376


 
How many raincoats can you sell in a day?
How many square yards of fabric do you need per thousand raincoats?
How many times do you plan to fold them?
How many years do you expect one to last?
Do you want breathable fabric, or nonporous fabric?
Do you have access to a cheap stream of polymer, film, or fabric?
Do you know anything about making film, fabric, or garments?
How much money can you spend before any comes in?

There's probably something intermediate between polyurethane coated nylon (heavy and expensive, but tough enough for inflatable powerboats), and cheesecloth between two plies of polyethylene film (possibly cheap, and basically disposable) that meets your needs, but you have to figure out what your needs are, hence the questions above. We don't need to know the answers, but you do.









Mike Halloran
Pembroke Pines, FL, USA
 
Mike

A large garbage or 50 gallon drum liner with 3 holes punched in the appropriate spot makes a real cheap plastic raincoat.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
kainebi

In addition to the good advice from Mike.

Do you mean plastic fibres woven into a raincoat, natural fibres woven then plastic coated or plastic film.



Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top