I have a valve which has been taken out from a clean propane gas service for inspection purposes. There is no corrosion but a mechanical failure upstream has left the valve covered with debris and dirt. Operations would like to water wash the valve using plant demineralized water before returning to service.
Valve has 316 body and operates around 40-50oC.
My fear is that the demin water may contain enough chlorides to cause chloride pitting corrosion when returned to service.
What precautions should be taken to water wash these valves?
What chloride content is acceptable for a demin water wash? I am seeing 50ppm and 100ppm max in API 510 and API 598 respectively.
Thanks
First time posting here so please be gentle
I have a valve which has been taken out from a clean propane gas service for inspection purposes. There is no corrosion but a mechanical failure upstream has left the valve covered with debris and dirt. Operations would like to water wash the valve using plant demineralized water before returning to service.
Valve has 316 body and operates around 40-50oC.
My fear is that the demin water may contain enough chlorides to cause chloride pitting corrosion when returned to service.
What precautions should be taken to water wash these valves?
What chloride content is acceptable for a demin water wash? I am seeing 50ppm and 100ppm max in API 510 and API 598 respectively.
Thanks