Hello
I have a question about your experience. I have a problem with micro contaminantion in my system (chlorination, 2 stages RO and EDI 6m ^ 3). The station works in two modes of circulation and production. During production, the water temperature is 10-12oC. During circulation, it is heated up to 22oC (production lasts almost 12 hours and circulation 12 hours). Do you think that if I add a cooling system (lower temp and circulation mode), it will help control the micro? Do any of you use such solutions?
 
What sort of microbiplogical contamination do you have?
I assume that you must be dechlorinating as well or is there another process that you don't mention?


Regards
Ashtree
"Any water can be made potable if you filter it through enough money"
 
Dropping the temperature is not going to control the contamination. Ask the supplier of your RO system for a recommendation on a biocide.
 