I have got two questions
1.How do we connect HDPE(high density poly-ethylene)pipe to brick masonry inspection chambers having masonry thickness 8.5" or 210mm-the joint should be leak-proof
2.An ordinary connection with out flange-joints filled with cement mortar(1:2 ratio) and also concreted (1:1.5:3) was found to have leak.How to rectify this problem?. [sig][/sig]
1.How do we connect HDPE(high density poly-ethylene)pipe to brick masonry inspection chambers having masonry thickness 8.5" or 210mm-the joint should be leak-proof
2.An ordinary connection with out flange-joints filled with cement mortar(1:2 ratio) and also concreted (1:1.5:3) was found to have leak.How to rectify this problem?. [sig][/sig]