The water for mold cooling? I has to be good enough so that you have clean piping so that flow is reliable, and the biggest one is to prevent scale formation on the hot molds.
It isn't super critical but controlling the pH, TDS, are scaling potential the keys.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed