Hello everybody
I have been designing a irrigation system, i shall install steel pipe for 20 first meters and the rest, 12 km, in GRP, so my doubt is: what happen in transition GRP-STEEL during a water hammer phenomen?
What's background for the majority of softwares for hydraulic transient analysis for this case?
The results seems no be real, because in the change of material the overhead up to 10 time the pressure, while in GRP is around 20%.
I'm not sure if i should use the concept: equivalent celerity.
I hope you can help me
Thanks in advance
César
I have been designing a irrigation system, i shall install steel pipe for 20 first meters and the rest, 12 km, in GRP, so my doubt is: what happen in transition GRP-STEEL during a water hammer phenomen?
What's background for the majority of softwares for hydraulic transient analysis for this case?
The results seems no be real, because in the change of material the overhead up to 10 time the pressure, while in GRP is around 20%.
I'm not sure if i should use the concept: equivalent celerity.
I hope you can help me
Thanks in advance
César