Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

water distribution pipe material 4

Status
Not open for further replies.

arj00

Civil/Environmental
Jan 7, 2003
13
What pipe material is preferable to use for water transmission line Dia. range 10inch- 16 inch.
Ductile iron is costly,GRP(glass reinforced plastic) is less costly but I did not use before! Do you think GRP is acceptable .
 
Replies continue below

Recommended for you

Good answer Hydrae.

In fact, HDPE will not hold roundness as well as others.

Lack of equipment is a problem too, although I find this less convincing because good equipment would be purchased if the customer perceived an advantage to switching to HDPE.

Poor quality of installation yes, good supervision by knowledgeable person is required. Installation error though is always there even with the others. I have seen operators out there with lead wool pounding the stuff into CI joints. C-900 I have seen not much but would suspect installation errors, hey, a fool can screw anything up.

PUMPDESIGNER
 