Any idea about pH or other impurities (Fe or Cu)?
We need more info.
The ferric chloride solution used in G48 C and D is 33,000ppm Cl and a pH of <0.5.
There are very few (very expensive) metals that will work at 100C in this.
Now if the pH were near neutral then superaustenitic, superferritic and superduplex grades might all become candidates.
If the pH is high then a superferritic would be the clear favorite.
= = = = = = = = = = = = = = = = = = = =
Plymouth Tube