reallyme00
Mechanical
- Dec 11, 2006
- 13
To All,
Recently I experienced a problem(Out board stationary ring crack) with my mechanical seal. The Outboard seal start to leak after two days of startup. leakage rate was 3drops/min. we found during dismantlig that the crack(near anti rotation pin groove) at the out board stationary ring caused the leak. The crack was hard to see ie., hair line crack.
The operator started the pump one day later, the instalation of the seal on the pump. At the inboard side there were symptoms that seal could have experienced high pressure(over pressurisation). The I/B seal contact pattern was like I.D contact and scratches at the outer circumference because of abrasive entry.
Now my question is, apart from instalation error what would cause this mating ring crack? I red one answer from Mr.JJPALIN, that cold start up could lead to crack of the hard face. Could I know more that How a cold start up could crack the mating ring? What are all the other possible causes?
your answers would help me to avoid the similar failures in future. I am sure that installation error is not an issue because we assembled the seal by taking the direction of rotation in mind.
Advance thanks to all.
Seal details:
It is a double mechanical ApI plan 02/53M seal.
RPM-2900, Pumping fluid Temp- 275 Deg C,
Stuffing box pr- 8 bar.
Barrier fluid pressure - 15 bar.
Barrier fluid temp - around 70 Deg C.
Stationary ring- silicon carbide
rotating ring - metal bellow with carbon face.
Recently I experienced a problem(Out board stationary ring crack) with my mechanical seal. The Outboard seal start to leak after two days of startup. leakage rate was 3drops/min. we found during dismantlig that the crack(near anti rotation pin groove) at the out board stationary ring caused the leak. The crack was hard to see ie., hair line crack.
The operator started the pump one day later, the instalation of the seal on the pump. At the inboard side there were symptoms that seal could have experienced high pressure(over pressurisation). The I/B seal contact pattern was like I.D contact and scratches at the outer circumference because of abrasive entry.
Now my question is, apart from instalation error what would cause this mating ring crack? I red one answer from Mr.JJPALIN, that cold start up could lead to crack of the hard face. Could I know more that How a cold start up could crack the mating ring? What are all the other possible causes?
your answers would help me to avoid the similar failures in future. I am sure that installation error is not an issue because we assembled the seal by taking the direction of rotation in mind.
Advance thanks to all.
Seal details:
It is a double mechanical ApI plan 02/53M seal.
RPM-2900, Pumping fluid Temp- 275 Deg C,
Stuffing box pr- 8 bar.
Barrier fluid pressure - 15 bar.
Barrier fluid temp - around 70 Deg C.
Stationary ring- silicon carbide
rotating ring - metal bellow with carbon face.