Can someone point me in the direction of a clause in ASME B31.3 where the visual acceptance limits change for high pressure lines?
We currently have a project where the acceptance refers to ASME B31.3 Table 341.3.2 & ASME V Article 9.
The WT is 10 and 11mm so the internal protrusion as I read it is below or equal to 3mm.
Our client is telling me that as this is a high pressure line and the acceptance is 1.5mm.
Having studied various chapters of ASME B31.3 I can not find this clause.
Is there one?
We currently have a project where the acceptance refers to ASME B31.3 Table 341.3.2 & ASME V Article 9.
The WT is 10 and 11mm so the internal protrusion as I read it is below or equal to 3mm.
Our client is telling me that as this is a high pressure line and the acceptance is 1.5mm.
Having studied various chapters of ASME B31.3 I can not find this clause.
Is there one?