Just a quick one, when inputing values into excel spreadsheet to calculate microvickers hardness ive noticed it to be about 50 points high. The machine is reading correct and also if i input the d1 and d2 values from the test block cert they also read around 50 points high. I dont see how this is possible because theres nothing in the calculation that could make it only slightly higher.
 
Replies continue below

Recommended for you


Are you using this equation?

HV = 1854.4 x P/d2

where:
P = force, gf
d = mean diagonal length of the indentation, μm
 