Does anyone have a reference discussing the effects (or lack thereof) of operating heavy construction equipment in the proximity of freshly-placed concrete?
 
Replies continue below

Recommended for you

See, "The vibration resistance of young & early age concrete." A. Ansell, J. Silfwerbrand. Dealing with pile driving and blasting, heavy machinery.
In: STRUCTURAL CONCRETE, Vol 4, Issue 3, Sept. 2003, P 125-134.
 
Thanks so much. I am working on getting a copy now. It looks like exactly what I am looking for.
 