Hi Everyone,
May someone know what type of this material (stainless steel or carbon steel) SA105 and SA-516 70 and the maximum and minimum temperature and Pressure for this steel?

Thank you.

Regards,

Shaga
 
Are you asking for someone to Google this for you??
 
Antonio .....

There seems to be some major concepts here that you do not understand.

- Pressure Vessels are engineered containers that are built to retain a specific liquid under the limitations of a maximum pressure and maximum temperature. The strength of the vessel depends both on the materials selected and the configuration of the vessel. Agreed-upon rules to design, test and certify a vessel are contained in something called a Pressure Vessel Code.

- Poorly designed pressure vessels have exploded and failed in the past. Many people have been killed

- Pressure Vessels are constructed from approved and tested materials. SA 105 and SA 516 are commonly used carbon steel pressure vessel materials.

- Because a pressure vessel is an engineered structure and therefore the (pressure retaining) strength depends on the materials AND configuration, we cannot answer your question.

Here is a place to start:



tell us more about your experience and what you are trying to do ....


MJCronin