What do you think is the cause for the vertical crack in the basement wall of single family home as shown below? It was discovered in several places of an 50 years old house.
It seems to be an old cracks but does not seems to be due to shrinkage or temperature. My first guess will be due to differential settlement over the years but not sure.
Thanks,
Alex
What do you think is the cause for the vertical crack in the basement wall of single family home as shown below? It was discovered in several places of an 50 years old house.
It seems to be an old cracks but does not seems to be due to shrinkage or temperature. My first guess will be due to differential settlement over the years but not sure.