I'm out on a plant in Egypt, the supplier has sent out some ball & gate valves with no tag/I.Ds on them & so I'm not sure which valve goes where.
I have some with a seat of A105N body, CR13HF, disc CR13HF, stem CR13
& some A105N body, F6 stem, F6 disc, F6HF seat, R35WB050
Which of these would be suitable for superheated steam at 16barg & 300degrees C??
Does anyone have a list of what these specifications mean, I have tried various web sites but come up with nothing.
Thanks