What is cause valve seat recession on LPG ?
How to reduce this problem?
Thank You!
Radek
What is cause valve seat recession on LPG ?
How to reduce this problem?
Thank You!
Radek
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
My bad, I should have wrote " pre-ignition contributes to valve recession through the excess heat transferred to the valve and valve seat insert, which may be already running on the ragged edge".turbocohen said:Winfieldblue, how does preignition "pound" valves into their seats