We need a recommendation for shut-off valves that will hold up to the rigors (H2S) of a sanitary effluent force main. Does anyone have experience with anything that is still working? We have epoxy coated butterfly and gate valves that become non-functional after a number of years due to H2S. We have already realized that the butterfly valves were a big mistake. Have heard some about eccentric plug valves with epoxy coating.

Steve
 
Replies continue below

Recommended for you

We prefer the Dezurik plug valves in our system.


PLUG VALVES

1. Type: Non-lubricated eccentric.
2. Rating: 150-psi W.O.G.
3. Ends: Flanged. Flanged valves are faced and drilled to ANSI/ASME B-16.42.
4. Laying Length: Through 12 inch, flange face-to-face dimensions equal to standard gate valves.
5. Body: Semi-steel with raised seats.
6. Seats: 4-inches and larger valves welded-in overlay of high nickel content on all surfaces contacting the plug face. Seat end of valve shall be on the side closest to the pump(s).
7. Plugs:
a. Resilient faced plugs.
b. Facings: Neoprene suitable for use with sewage, sludge or scum.
c. Port areas for 20-inch valves: At least 80-percent of full pipe area.
8. Bearings: Valves through 20-inches shall have permanently lubricated stainless steel bearings in the upper and lower plug stem journals.
9. Bonnet: Bolted.
10. Packing 4-inches and larger valves:
a. Repacked without removing the bonnet.
b. Adjustable.
11. Zinc Plating: All exposed nuts, bolts, springs and washers.
12. Plug valves 6-inches and larger shall be provided with gear operators attached to valve. Plug valves smaller than 6-inches shall be provided with factory supplied levers.
13. Manufacturer: DeZurik.
 