HI,
I have a proposal for valve components material for butterfly valve which i need to replace. application is seawater , max pressure 10 bar , temperature ambient (0-60C)
these are the material options:
Body
uctile iron with EPDM internal liner
Shaft: dry shaft with SS 420
Disc: Ebonite coated Ductile Iron
Seat: EPDM
Are these good material options for my application. when it comes to strength & corrosion resistance. Can anyone advise from experience please?
Thank you
I have a proposal for valve components material for butterfly valve which i need to replace. application is seawater , max pressure 10 bar , temperature ambient (0-60C)
these are the material options:
Body

Shaft: dry shaft with SS 420
Disc: Ebonite coated Ductile Iron
Seat: EPDM
Are these good material options for my application. when it comes to strength & corrosion resistance. Can anyone advise from experience please?
Thank you