HI All,

To calculate thickness of the pipe. I am looking for the values of coeffiicent (Y)for Inconel 600 and Inconel 625. ASME B313.3 list the Y vaues for Ferritic steels and some others but not for nickel alloys.

Can anyone help me out.

Thanks in advance.

Asif Raza
 
did you try google?

regards,
roker
 
Table 304.1.1 specifies 0.4 for "other ductile materials" so that is what you have to use.
 
Thanks a lot guys for your help.

Asif