For our application (a vacuum tight tank) we need to have a welding connection with a very high gas leaking tightness. What kind of welding technology is suitable for high vacuum tightness? Our requirement is a leaking tightness below 150 * 10-9 mbar * dm3 / s (for air) for a 10 dm3 volume tank. The length of the total weld is approximately 2 meter (the form of the tank is very slim). What kind of gas tightness is possible for welding connection for industrial applications?
 
Replies continue below

Recommended for you

If done properly by a skilled welder the weld proper will have the same permeability as the base metal, "O" except to Helium and Hydrogen. It's the defects in the weld that cause problems. Skilled welders and through inspection will take the weld out of the picture.

All high vacuum equipment use welding.
 
Skillful TIG welding joints that are not very constrained works pretty good in stainless steel
 