I need to design a graphite fixture.

I see there is several diffrent grades of graphite
Please advise which grade should be used.
it of course needs to be flat.

not sure what grades can be run in a vacuum furnace.

Thanks for you help in advance.
 
Replies continue below

Recommended for you

Why not go ask semiconductor processing equipment suppliers?