Hello all,

I have below one question that may be very silly but i am stuck to find the answer.

"UW-16(f)(2) stated that:"(2) Fittings not exceeding NPS 3 (DN 80) shown on Figure UW-16.1, sketches (x), (y), (z), (aa), and (bb) may be attached by welds that are exempt from size requirements with the following limitations"

I have question what is meaning of "that are exempt from size requirements" in the above clause.

Thanks in Advance
 
Replies continue below

Recommended for you

Jagmtr, the weld sizing requirements are shown in the various sketches; example "t1 + t2 >= 1 1/4 tmin". The welds may be exempt form this requirement subject to rules in (f)(2)(-a) & (-b).

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
I was thinking same but was not sure. Thanks SnTMan for your kind response
 
Of course. Best of luck :)

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 