Am I required to follow the rules of UW-13.1 if I am welding a hemispherical head directly to an Appendix 2 weld neck flange? (my nominal head thk is less than my flange hub thk)

Thanks
 
Replies continue below

Recommended for you

If you are butt welding the head to the flange you need to refer to the fig UW-9 to provide the necessary transition taper.

What type joint are you considering?

Is your head sized for the same pipe size as the flange?
 