Jan 16, 2004 #1 nbucska Electrical Joined Jun 1, 2000 Messages 2,191 Location US Transparent, lowcost UV resistant plastic? <nbucska@pcperipherals.com>
Jan 16, 2004 #2 patprimmer New member Joined Nov 1, 2002 Messages 13,816 Location US PMMA, Acrylic, Methyl Methacrylate. Regards pat Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
PMMA, Acrylic, Methyl Methacrylate. Regards pat Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
Jan 19, 2004 #3 plasticsguru Materials Joined Mar 15, 2002 Messages 16 Location US ASA is also a good choice. Also materials that are average in UV can be modifed with the addition of additives to make them more UV resistant. Upvote 0 Downvote
ASA is also a good choice. Also materials that are average in UV can be modifed with the addition of additives to make them more UV resistant.
Jan 19, 2004 #4 Soupcat Mechanical Joined Aug 28, 2002 Messages 76 Location IE Not to forget PC...for extra strenghth and toughness. ASA is marketed on it's ability to retain colour. It has exceptional colour fastness properties and won't fade much over time even in direct sunlight. Kieran http://www.moulddesigner.com Upvote 0 Downvote
Not to forget PC...for extra strenghth and toughness. ASA is marketed on it's ability to retain colour. It has exceptional colour fastness properties and won't fade much over time even in direct sunlight. Kieran http://www.moulddesigner.com
Jan 19, 2004 #5 patprimmer New member Joined Nov 1, 2002 Messages 13,816 Location US nbucska My original answer was as brief as your question. If you want more info, please elaborate, particularly re application and environment of use. Regards pat Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
nbucska My original answer was as brief as your question. If you want more info, please elaborate, particularly re application and environment of use. Regards pat Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
Jan 28, 2004 Thread starter #6 nbucska Electrical Joined Jun 1, 2000 Messages 2,191 Location US Thanks, Pat. <nbucska@pcperipherals.com> Upvote 0 Downvote